Cotreatment of flotation waste, neutralization sludge ...
· Firstly, the preparation parameters of binder composed of FWCS, NS, and cement clinker were optimized to be FWCS dosage of 40%, NS dosage of 10%, cement clinker dosage of 50%, mill time of h, and watertobinder ratio of On these conditions, the unconfined compressive strength (UCS) of the binder reached MPa after hydration of 28 days. Then, the binder was used to .